MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total 7823MZ Polypropylene, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: High flow clarified random copolymer for injection molding

Clarity - FINA 7823MZ exhibits superior clarity and produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.

Antistat - FINA 7823MZ contains an antistat to help protect molded parts from dust accumulation.

Easy Flow - FINA 7823MZ exhibits exceptionally easy flow characteristics.

FDA - FINA 7823MZ complies with all applicable FDA and USDA regulations and may be used under these provisions for food contact and packaging.

Recommended Applications - FINA 7823MZ is recommended for injection molding housewares, cassette cases and other items calling for good impact and superior clarity.

Processing - FINA 7823MZ resin processes on conventional injection molding equipment with typical melt temperatures of 350-450°F (177-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 30 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 84ASTM D288A
Hardness, Shore D 76ASTM D1706
Tensile Strength, Ultimate 29.7 MPaASTM D638
Elongation at Break 11 %ASTM D638
Modulus of Elasticity 1.10 GPaASTM D638
Flexural Modulus 0.965 GPaASTM D790
Izod Impact, Notched 0.740 J/cmASTM D256A
Izod Impact, Unnotched NBASTM D256A
Impact Test 17.5 J
@Thickness 3.17 mm
Drop Impact, plaques. Fina API test
 
Thermal PropertiesOriginal ValueComments
Melting Point 145 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 177 - 232 °CInjection
 
Compliance PropertiesOriginal ValueComments
USDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin (European Grade)
Borealis HL504FB Polypropylene Homopolymer
A. Schulman PP 3476 Polypropylene Homopolymer, Fiber Grade
Total 7235 Polypropylene, Blow Molding Grade
Total 3829 Polypropylene, Injection Molding Grade

PFINA1 / 38431

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.