MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makroblend® AR205 PC+PET
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: (PC+PET) blend, easy flow, impact modified; application: automotive body panels

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183-1
Viscosity 200 cP
@Frequency 1000 Hz,
Temperature 270 °C
b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm150x105x3 mm; 270 °C / MT 70°C; 600 bar; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm150x105x3 mm; 270 °C / MT 70°C; 600 bar; b.o. ISO 2577
Melt Flow 38 g/10 min
@Load 5.00 kg,
Temperature 270 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 48.0 MPa50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 45.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 4.8 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2200 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 80.0 MPa2 mm/min; ISO 178
Flexural Yield Strength 68.0 MPa
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2200 MPa2 mm/min; ISO 178
Flexural Strain at Yield 5.8 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²
@Temperature -30.0 °C
ISO 180-A
 45.0 kJ/m²
@Temperature 23.0 °C
ISO 180-A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ISO 180-1C
 NB
@Temperature -30.0 °C
ISO 180-1C
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 NB
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched 20.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 45.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
Impact 3900
@Temperature 23.0 °C
[N], Puncture Max Force; ISO 6603-2
 5000
@Temperature -30.0 °C
[N], Puncture Max Force; ISO 6603-2
Puncture Energy 42.0 J
@Temperature 23.0 °C
ISO 6603-2
 48.0 J
@Temperature -30.0 °C
ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 81.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 82.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 126 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °CISO 75-1,-2
Vicat Softening Point 138 °C
@Load 5.10 kg
120°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °CISO 294
Mold Temperature 70.0 °CISO 294
Injection Velocity 200 mm/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makroblend® UT250 HR PC+PET
Covestro Makroblend® UT203 PC+PET
Covestro Makroblend® UT235 M PC+PET
Covestro Makroblend® M525 PC+PET
Covestro Makroblend® UT6007 PC+PBT

PCOVEST0797 / 202580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.