MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NatureWorks® Ingeo™ 6202D Fiber Grade PLA
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically drawn staple fibers using conventional fiber spinning and drawing equipment. NatureWorks® PLA 6202D can be converted into a broad range of fiber products and is recommended for non-dyed fiber applications. Potential applications for PLA polymer 6202D include: Fiberfill; Non-wovens; Agricultural woven and nonwoven fabrics; Articles for household disposal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Melt Density 1.08 g/cc
@Temperature 230 °C
ASTM D1238
Viscosity Measurement 3.1Relative Viscosity; CD Internal Viscotek Method
Melt Flow 15 - 30 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 10 - 70 %Fiber; ASTM D2256/ASTM D3822
Tenacity 2.50 - 5.00 g/denierASTM D2256/ASTM D3822
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 170 °CASTM D3418
Glass Transition Temp, Tg 55.0 - 60.0 °CASTM D3417
Shrinkage <= 8.0 %
@Temperature 130 °C,
Time 600 sec
Hot Air; ASTM D2102
 
Processing PropertiesOriginal ValueComments
Drying Temperature 80.0 °C
@Time 14400 sec
Dew Point -35.0 °C
Drying Air Flow Rate >= 0.500 ft³/min (CFM)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer
Braskem PB681/59 LDPE Blown Film Extrusion Polyethylene
Braskem PB681/59 Blown Film Extrusion Low Density Polyethylene
Braskem PB681 LDPE Cast and Blown Film Extrusion, Injection Molding Polyethylene
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene

PNATU93 / 103491

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.