MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont 20 Series 2020 Specialty Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization process, have a well earned reputation for processability and outstanding flexibility and environmental stress crack resistance. DPE 2020T and 2020 are identical products with DPE 2020T passing a "tube defect" specification that is not required for DPE2020.

Typical Applications: Extruded squeeze tubes for personal care, cosmetic, and pharmaceutical applications; Tube shoulders providing headers for LDPE, HDPE and coextruded squeeze tubes; Low pressure water and air tubing; Rotational molding fittings; Molding of small bottles, caps, seals, etc. for medical, personal care and other applications.

Features & Benefits: Superior resistance to environmental stress cracking; High flexibility; Good heat stability; Excellent color; Odor free; Excellent chemical resistance; Tasteless; Nontoxic.

Each lot of DPE 2020T passes an internal tube imperfection specification.

Information provided by DuPont Packaging Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D792
Melt Flow 1.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 51ASTM D2240
Tensile Strength, Ultimate 18.6 MPaASTM D638
Tensile Strength, Yield 9.60 MPaASTM D638
Elongation at Break 620 %ASTM D638
Modulus of Elasticity 0.186 GPaASTM D638
Flexural Modulus 0.238 GPaASTM D790
Izod Impact, Notched NBASTM D256
 0.430 J/cm
@Temperature -40.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 93.0 °CFreezing Point via DSC/ASTM D3418
 109 °CUpon Melting via DSC/ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °CASTM D648
Vicat Softening Point 97.0 °CASTM D1525
Brittleness Temperature <= -76.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.51ASTM D542
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 193 °CTypical die temp for tube extrusion.
Melt Temperature 188 °Ctube extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont 20 Series DPE 20 Specialty Polyethylene Resin
Chevron Phillips Marlex® HHM 5502-01 ST High Density Ethylene Hexene Copolymer
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer
Celanese Hostaform® C 2521 XAP² ™ POM, Unfilled
Aaron Industries AVPE HD 300-3 MELT 20 Virgin Polyethylene

PDUPF2 / 33599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.