MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M S32HS Glass Bubbles
Categories: Ceramic; Glass

Material Notes: 3M™ Glass Bubbles S32HS are high-strength, low-density additives specially formulated to afford greater survivability than other lightweight additives under demanding processing conditions. They are hollow glass microspheres made from water-resistant and chemically-stable soda-lime borosilicate glass. These hollow glass microspheres can be used as a low-density filler material for many applications. 3M glass bubbles help to reduce weight; reduce noise, vibration and harmonics; reduce thermal expansion; and contribute to cost savings. They are used in a variety of applications in diverse markets, including automotive, construction materials, electronics, marine and paints and coatings.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 g/cc
Volatiles 0.50 %
Particle Size 25 µmAverage diameter
 47 µmD95
pH 9.5at 5 wt% loading in water
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 6000 psi90% survival by volume
 
Thermal PropertiesOriginal ValueComments
Softening Point 600 °C
 
Descriptive Properties
AppearanceOff-white, powderyunaided eye
Compositionsoda-lime-borosilicate glass
ShapeHollow spheres with thin walls

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33063A / 255388

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.