MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Go Yen Chemical GOYENCHEMUV-3000 Light Absorber
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS NO. 131-56-6

GOYENCHEMUV-3035 is a highly effective anti-UV product which has an excellent anti-UV effect and thermal stability especially on plastics, coatings, ink, and adhesives.

Advantages:

  • light color
  • good compatibility
  • easy to processing
Applications:
  • Polyethylene
  • Polypropylene
  • Polystyrene
  • AS resin
  • ABS resin
  • Polycarbonate
  • Polyvinyl chloride
  • Polyvinylidene chloride
  • Polyester
  • Polyamide

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 214.2 g/mol214.2 g/mol
Ash <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 142 - 146 °C288 - 295 °F
 
Optical PropertiesMetricEnglishComments
UV Transmittance  >= 95 %
@Wavelength 450 nm
>= 95 %
@Wavelength 450 nm
 >= 97 %
@Wavelength 500 nm
>= 97 %
@Wavelength 500 nm
 
Descriptive Properties
AppearanceYellow crystalline powder
Loss on drying<0.5%
Purity=99%HPLC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN565 / 266873

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.