MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Crosslinker OX 20
Categories: Other Engineering Material

Material Notes: Crosslinker OX are oxime silane-based crosslinkers for producing neutral moisture-curing silicone sealants. Using these silane compounds, hydroxy-functionalized silicone polymers are crosslinked to obtain a silicone elastomer under the effect of a catalyst and moisture. When using Crosslinker OX, no acetic acid or amine is released in contrast to acid or alkaline crosslinking systems, but 2-butanone oxime. As this cleavage product reacts neutrally, sealing compounds based on Crosslinker OX can be used even on sensitive substrates such as marble.

Application: Crosslinker OX is used in sealants, usually at concentrations of between 4 and 6 wt%. The various Crosslinker OX differ by their reactivity, with the general rule being:
TOS > VOS > MOS
Mixing different Crosslinker OX types enables setting the rate of a formulation precisely, i. e. skin-over time, curing rate and time to first elastic recovery.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/cc
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.455 - 1.483
 
Descriptive Properties
Appearanceclear, colorless to yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIL777 / 196981

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.