This nuance of nickel preserves all the particularities of pure nickel but has been light strengthened with an addition of manganese. This is mainly used for cold connections but also for electrical and electronic applications such as lead wires, supporting components in lamps and cathode-ray tubes, and electrodes in glow discharge lamps.Information provided by Aperam |