MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling SUSTAMID® 66 FG PA 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Product characteristics:
  • Good dimensional stability
  • Very good sliding properties
  • Suitable for contact with foodstuffs according to (EC) No. 1935/2004
Product applications:
  • Mechanical engineering
  • Food processing industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccDIN EN ISO 1183-1
Water Absorption 2.8 %DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83DIN EN ISO 868
Tensile Strength, Yield 85.0 MPaDIN EN ISO 527
Elongation at Break 50 %DIN EN ISO 527
Modulus of Elasticity 3.00 GPaDIN EN ISO 527
Izod Impact, Notched (ISO) 3.00 kJ/m²DIN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDIN EN 62631-3-1
Surface Resistance 1.00e+13 ohmDIN EN 62631-3-2
Dielectric Constant 3.8IEC 60250
Dielectric Strength 25.0 kV/mmIEC 60243
Dissipation Factor 0.015
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CDIN 53752
Specific Heat Capacity 1.70 J/g-°CDIN 52612
Thermal Conductivity 0.230 W/m-KDIN 52612-1
Melting Point 260 °CISO 11357-3
Maximum Service Temperature, Air 95.0 °Clong term
 170 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 100 °CDIN EN ISO 75
Minimum Service Temperature, Air -30.0 °C
Flammability, UL94 HB
@Thickness 3.00 mm
 V-2
@Thickness 6.00 mm
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ 101 / Ertalon™ 66 SA PA66 Extruded, Unfilled, Type 66 Natural and Black
EPICHEM PA 66 Polyamide 66
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass
EPICHEM Epinyl PA 66 Polyamide 66
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned

PROCH9303 / 233005

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.