Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) black 9922 main characteristics are the following properties:- high heat aging resistance
- excellent surface finish
- easy processibility
- high stiffness and impact strength even after long-term heat tempering
Grilon B XE 5026 (BG-30 H) black 9922 main attributes are to be shown for the production of parts with high needs on temperature resistance with highest demands on temperature resistance, for example parts like applications in engine rooms of vehicles.Information provided by EMS Grivory. |