MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2800 B-45A Z Thermoplastic Polyolefin Elastomer (TEO) FDA Compliant Ingredients
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 4610 s delay; ASTM D 2240
Tensile Strength at Break 530 psi
@Thickness 3.20 mm
Die C; 20 in/min (500 mm/min); ASTM D 412
Tensile Stress at Strain 170 psi
@Strain 100 %,
Thickness 3.20 mm
Die C; 20 in/min (500 mm/min); ASTM D 412
Elongation at Break 450 %
@Thickness 3.20 mm
Die C, 20 in/min (500 mm/min); ASTM D 412
Tear Strength 90.0 pliDie C; ASTM D 624
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 440 °F
Mold Temperature 50.0 - 175 °F
Drying Temperature 175 °F
@Time 7200 - 10800 sec
Moisture Content <= 0.080 %
Dew Point 0.000 °F
Injection Pressure 10000 - 15000 psi
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Barlog Plastics KEBAFLEX S 45 A.01 TPE-S, Shore A45, translucent
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
Dynasol Solprene® 412 Thermoplastic Elastomer

PQZSA8655 / 178122

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.