MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics ParPHorm® S1945-25 Non-Conductive Form-in-Place Gasket
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material cost versus performance and can provide low cost alternatives for less demanding applications. Chomerics corrosion resistant materials inherently provide protection against galvanic activity. They may eliminate the need for nickel or tin plating and or secondary environmental gaskets. Chomerics general purpose materials exhibit excellent electrical and mechanical properties on metallic and shield plastic housing. Chomerics silver filled materials provide high shielding and conductivity critical for inter-compartmental shields.

Features: Lower deflection forces and a broad deflection range, Corrosion resistant materials can eliminate plating or secondary environmental gasket, Good adhesion to many substrates, Supply chain management providing ongoing logistics, and Low cost and rapid prototyping.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.780 g/cc0.780 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525ASTM D2240
Tensile Strength >= 1.91 MPa>= 277 psiASTM D412
Elongation at Break 316 %316 %ASTM D412
Compression Set  21 %
@Temperature 70.0 °C,
Time 252000 sec
21 %
@Temperature 158 °F,
Time 70.0 hour
ASTM D395
 42 %
@Temperature 100 °C,
Time 252000 sec
42 %
@Temperature 212 °F,
Time 70.0 hour
25% deflection; ASTM D395
 
Processing PropertiesMetricEnglishComments
Cure Time  1800 min
@Temperature 140 °C
30.0 hour
@Temperature 284 °F
Handling Time
 1800 min
@Temperature 140 °C
30.0 hour
@Temperature 284 °F
Full Cure
Tack-Free Time 1800 min
@Temperature 140 °C
30.0 hour
@Temperature 284 °F
 
Descriptive Properties
ColorDark Grey
Resin SystemSilicone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME214 / 130924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.