MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® US 5544 Two-Component Flexible, Flame Retardant, Polyurethane Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Loctite Stycast US 5544 provides the following product characteristics: Room temperature cure

Application: Potting and Encapsulating

Loctite Stycast US 5544 is a fast gelling, flexible, flame retardant, mineral-filled, polyurethane compound. Loctite Stycast US 5544 is a fast-setting potting compound which is low in viscosity, therefore flows well and adheres well to many substrates. It has very low odor and does not contain TDE or mercury compounds.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccPart A
 1.40 g/ccMixed
 1.46 g/ccPart B
Water Absorption 0.15 %
@Time 86400 sec
Viscosity 75 cPPart A
 2000 cPMixed
 11000 cPPart B
Linear Mold Shrinkage 0.0012 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79 - 89
Tensile Strength 1320 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.60e+13 ohm-cm
Dielectric Constant 3.85
@Frequency 100 Hz
Dielectric Strength >= 400 V/mil
Dissipation Factor 0.020
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 114 µm/m-°C
@Temperature -40.0 - 25.0 °C
Alpha 1
 155 µm/m-°C
@Temperature 25.0 - 125 °C
Alpha 2
Thermal Conductivity 0.335 W/m-K
Flammability, UL94 V-2
@Thickness 6.35 mm
 V-0
@Thickness 9.52 mm
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 60.0 - 85.0 °C
Alternate
 2.00 - 4.00 hour
@Temperature 23.0 °C
Recommended
Working Life 2.00 - 3.00 min
Gel Time 4.00 - 6.00 min
 
Descriptive Properties
AppearanceClear BrownComponent A, Resin
 Opaque WhiteComponent B, Hardener
 Opaque WhiteMixed
Mix Ratio, by Volume1 : 4.81Part A : Part B
Mix Ratio, by Weight15 : 85Component A : Component B
Weight Loss (%)0.19Weight Loss after 168 hrs @ 130ºC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7971 / 255455

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.