MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
AFE Technologies Cronite 25Cr/20Ni No. HR6
Categories: Metal; Superalloy; Iron Base

Material Notes: High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.

Information provided by AFE Technologies/North American Cronite, Inc.

Key Words: Cronite 25/20; Werkstoff 1.4848; ASTM A297-HK
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 500 MPaAs Cast
Tensile Strength, Yield 260 MPaAs Cast
Elongation at Break 12 %As Cast; 5.65 A0.5
Rupture Strength 2.20 MPa
@Temperature 1150 °C,
Time 3.60e+7 sec
Stress Rupture
 3.80 MPa
@Temperature 1100 °C,
Time 3.60e+7 sec
Stress Rupture
 6.00 MPa
@Temperature 1050 °C,
Time 3.60e+7 sec
Stress Rupture
 9.50 MPa
@Temperature 1000 °C,
Time 3.60e+7 sec
Stress Rupture
 14.5 MPa
@Temperature 950 °C,
Time 3.60e+7 sec
Stress Rupture
 21.0 MPa
@Temperature 900 °C,
Time 3.60e+7 sec
Stress Rupture
 30.0 MPa
@Temperature 850 °C,
Time 3.60e+7 sec
Stress Rupture
 41.0 MPa
@Temperature 800 °C,
Time 3.60e+7 sec
Stress Rupture
 55.0 MPa
@Temperature 750 °C,
Time 3.60e+7 sec
Stress Rupture
 72.0 MPa
@Temperature 700 °C,
Time 3.60e+7 sec
Stress Rupture
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 25 %
Iron, Fe 52.1 %As Remainder
Manganese, Mn 1.0 %
Nickel, Ni 20 %
Silicon, Si 1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cunife® Hard Magnetic Alloy
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested longitudinal, round bar 75 mm
446 Stainless Steel, Annealed Sheet
410 Cb Martensitic Stainless Steel (UNS S41040)
405 Stainless Steel, annealed, bar

NCRON01 / 15986

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.