The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybdenum disulphide results in an improved crystalline structure enhancing bearing and wear properties. - High mechanical strength, stiffness, hardness and toughness
- Good fatigue resistance
- High mechanical damping ability
- Good sliding properties
- Excellent wear resistance
- Good electrical insulating properties
- Good resistance to high energy radiation (gamma- and X-rays)
- Good machinability
Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials. |