MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin DAI-EL® G-8002 Fluoroelastomer Terpolymer, 66% Fluorine Content  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-8002 is a peroxide curable copolymer designed for injection molding. DAI-EL® G-8002 can be formulated with various peroxide cure systems and can be used for co-extrusion with other elastomers. DAI-EL® G-8002 provides superior mechanical properties. In comparison to bisphenol cured fluoroelastomers, this material gives better resistance to steam and aqueous solutions.

Typical Applications: Turbo charge hoses, fuel hoses, gaskets, O-rings, seals

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.81 g/cc1.81 g/cc
Mooney Viscosity 25
@Temperature 121 °C
25
@Temperature 250 °F
ML 1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7171
Tensile Strength at Break 21.9 MPa3180 psi
 23.2 MPa
@Treatment Temp. 200 °C,
Time 252000 sec
3360 psi
@Treatment Temp. 392 °F,
Time 70.0 hour
Air Oven Aging
Elongation at Break 350 %350 %
 347 %
@Treatment Temp. 200 °C,
Time 252000 sec
347 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Air Oven Aging
100% Modulus 3.50 MPa
@Strain 100 %
508 psi
@Strain 100 %
Compression Set  4.0 %
@Temperature 175 °C,
Time 252000 sec
4.0 %
@Temperature 347 °F,
Time 70.0 hour
#214 O-ring; ASTM D395 Method B
 12 %
@Temperature 200 °C,
Time 252000 sec
12 %
@Temperature 392 °F,
Time 70.0 hour
#214 O-ring; ASTM D395 Method B
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -19.0 °C-2.20 °FLow Temperature Retraction; ASTM D1329
 
Processing PropertiesMetricEnglishComments
Cure Time 0.460 min0.00767 hourts2, scorch time
 0.590 min0.00983 hourt'50, time to 50% cure
 0.780 min0.0130 hourt'90, time to 90% cure
 10.0 min
@Temperature 177 °C
0.167 hour
@Temperature 351 °F
Press Cure
 240 min
@Temperature 200 °C
4.00 hour
@Temperature 392 °F
Post cure
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 66 %66 %
 
Descriptive Properties
ColorWhite to pale brown
MH22.9 dNmmaximum torque
ML0.5 dNmminimum torque
Test Formula100 phrDAI-EL® G-8002
 3 phrPeroxide (50% Activity)
 3 phrZinc Oxide
 30 phrMT Carbon Black (N-990)
 4 phrTAIC (72% Activity)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIJ9856 / 209927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.