System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Network Polymers SAN 279 Water White Color
Categories:
Polymer
;
Thermoplastic
;
SAN Polymer
;
Styrene Acrylonitrile (SAN), Transparent
Material Notes:
Description:
SAN - Styrene Acrylonitrile Transparent Engineering Thermoplastic
Information provided by Network Polymers Inc.
A. Schulman has acquired Network Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.08
g/cc
1.08
g/cc
ASTM D792
Linear Mold Shrinkage
0.0030
-
0.0070
cm/cm
0.0030
-
0.0070
in/in
ASTM D955
Melt Flow
2.0
g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.0
g/10 min
@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
7.5
g/10 min
@Load 3.80 kg,
Temperature 230 °C
7.5
g/10 min
@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
123
123
ASTM D785
Tensile Strength, Yield
71.7
MPa
10400
psi
chs 2 in/min; ASTM D638
Flexural Modulus
3.45
GPa
500
ksi
Tangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched
0.214
J/cm
0.400
ft-lb/in
0.125 inch bar; ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
88.9
°C
192
°F
Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Vicat Softening Point
101
°C
214
°F
0.125 inch bar, 1 Kg; ASTM D1525
Flammability, UL94
HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
Optical Properties
Metric
English
Comments
Haze
1.9 %
1.9 %
ASTM D1003
Transmission, Visible
89 %
89 %
ASTM D1003
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PDIAM031 / 29869
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.