MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
X12CrNi177 Austenitic Stainless Steel for medical instruments
Categories: Metal; Ferrous Metal; Austenitic; Special-Purpose Steel; Stainless Steel

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 515 MPaAnnealed
 1280 MPaFull hard
Tensile Strength, Yield 205 MPaAnnealed
 965 MPaFull hard
Elongation at Break 9.0 %Full hard
 40 %Annealed
Modulus of Elasticity 193 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 70.0 - 300 °C
Specific Heat Capacity 0.500 J/g-°C
Thermal Conductivity 16.2 W/m-K
 
Descriptive Properties
Magnetic PropertiesParamagnetic

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for T 600 Series Stainless Steel
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel, condition H1025
BASF Ultramid® A3EG7 BK00564 35% Glass Filled PA66 (Dry)
BASF Ultramid® A3K BK00464 PA66 (Dry)
BASF Ultramid® A3X2G5 BK23187 25% Glass Filled PA66 (Dry)

MMEDIC05 / 12381

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.