MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 8001-H18
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Other Wrought Al Alloy

Key Words: UNS A98001; Aluminium 8001-H18; AA8001-H18; Al8001-H18
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.75 g/ccEstimated from trends in similar Al alloys.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 54500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 69Converted from Brinell Hardness Value
Tensile Strength, Ultimate 200 MPa
Tensile Strength, Yield 185 MPa
Elongation at Break 4.0 %In 5 cm; Sample 1.6 mm thick
Modulus of Elasticity 70.0 GPaAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus. Estimated from trends in similar Al alloys.
Poissons Ratio 0.33Estimated from trends in similar Al alloys.
Shear Modulus 26.0 GPaEstimated from similar Al alloys.
Shear Strength 120 MPaCalculated value.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 24.0 µm/m-°C
@Temperature 20.0 °C
Estimated from trends in similar Al alloys.
 25.5 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.880 J/g-°CEstimated from trends in similar Al alloys.
Melting Point <= 650 °CEstimated from trends in similar Al alloys.
Liquidus 650 °CEstimated from trends in similar Al alloys.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 98.3 %As remainder
Boron, B <= 0.0010 %
Cadmium, Cd <= 0.0030 %
Cobalt, Co <= 0.0010 %
Copper, Cu <= 0.15 %
Iron, Fe 0.45 - 0.70 %
Lithium, Li <= 0.0080 %
Nickel, Ni 0.90 - 1.3 %
Silicon, Si <= 0.17 %
Zinc, Zn <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 8001-O
8005 Aluminum Composition Spec
Aluminum 2011-T6
Aluminum 7475-T61 (Extended High Temperature Data)
Aluminum 5042-H19

MA8001H18 / 9655

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.