MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.001" Diameter Wire, Allycarbonate EMI Shielding Window
Categories: Polymer

Material Notes: Description: Tecknit Allylcarbonate shielded windows are manufactured by casting a woven EMI shield mesh into a material that has optical properties similar to that of glass. The window offers a lightweight, cost effective alternative to traditional glass laminated shielded windows and is a more flexible material to machine, making it more suited to meet the changing design demands that are part of modern electronics.

Application Information: Allylcarbonace windows are ideally suited to applications where there is a requirement to shield displays or visual apertures. Windows are machined using computerized programming technology

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 97ASTM D785
 
Electrical PropertiesOriginal ValueComments
Shielding Effectiveness 35 dB
@Frequency 1e+10 Hz
Plane Wave
 40 dB
@Frequency 100000 Hz
H-Field
 52 dB
@Frequency 1e+9 Hz
Plane Wave
 105 dB
@Frequency 1e+7 Hz
E-Field
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
 130 °C1 hour duration
Minimum Service Temperature, Air -60.0 °C
 -60.0 °C1 hour duration
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 93.3 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME396 / 131106

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.