MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ FE 5642 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dyneon™ Fluoroelastomer FE 5642 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FE 5642 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability.
  • Composition: Di-polymer of vinylidene fluoride and hexafluoropropylene
  • Process targets: transfer and compression molding, bonding and calendering
  • Improved scorch resistance at high molding temperatures
  • Proprietary incorporated cure technology
  • Excellent mold release
  • Targeted for bonding shaft seal applications
  • Clean running

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/cc
Mooney Viscosity 42
@Temperature 121 °C
42
@Temperature 250 °F
ML1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7272Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 17.4 MPa2530 psiPress Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 230 %230 %Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 4.90 MPa
@Strain 100 %
710 psi
@Strain 100 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 17 %
@Temperature 200 °C,
Time 252000 sec
17 %
@Temperature 392 °F,
Time 70.0 hour
O-rings -214; ASTM D395 Method B
 
Thermal PropertiesMetricEnglishComments
Transformation Temperature -18.0 °C-0.400 °FTR10; ASTM D1329
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 65.9 %65.9 %
 
Descriptive Properties
ColorOpaque Off-White
MH, Maximum Torque17.6 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
 18.2 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 200°C
ML, Minimum Torque1.2 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 200°C
 1.5 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
SolubilityKetones and Esters
t`50, Time to 50% cure0.7 minutes100 cpm, 0.5° Arc, 6 Minutes @ 200°C
t`50, Time to 50% cure 2.1 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure @ 177°C - 3.3 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure @ 200°C - minutes1 minutes100 cpm, 0.5° Arc, 6 Minutes @ 200°C
ts2 - Time to 2 in-lb rise from min0.6 minutes100 cpm, 0.5° Arc, 6 Minutes @ 200°C
 1.6 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDYNE130 / 34938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.