MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 2RK65 HV Strip steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sandvik 2RK65 HV is a vacuum arc remelted high alloy austenitic stainless steel with very high cleanliness resulting in good polishability. The grade is also characterized by very good overall corrosion resistance and good weldability.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 160
Tensile Strength, Ultimate 520 - 720 MPa
Tensile Strength, Yield >= 25.0 MPa
@Strain 1 %
 >= 230 MPa
@Strain 0.2 %
Elongation at Break 35 %
Modulus of Elasticity 158 GPa
@Temperature 500 °C
 166 GPa
@Temperature 400 °C
 174 GPa
@Temperature 300 °C
 182 GPa
@Temperature 200 °C
 190 GPa
@Temperature 100 °C
 195 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000940 ohm-cm
@Temperature 20.0 °C
 0.00000990 ohm-cm
@Temperature 100 °C
 0.0000107 ohm-cm
@Temperature 200 °C
 0.0000113 ohm-cm
@Temperature 300 °C
 0.0000115 ohm-cm
@Temperature 400 °C
 0.0000115 ohm-cm
@Temperature 600 °C
 0.0000117 ohm-cm
@Temperature 500 °C
 0.0000118 ohm-cm
@Temperature 700 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.5 µm/m-°C
@Temperature 30.0 - 100 °C
 16.0 µm/m-°C
@Temperature 30.0 - 200 °C
 16.5 µm/m-°C
@Temperature 30.0 - 300 °C
 17.0 µm/m-°C
@Temperature 30.0 - 400 °C
 17.0 µm/m-°C
@Temperature 30.0 - 500 °C
 17.5 µm/m-°C
@Temperature 30.0 - 600 °C
 17.5 µm/m-°C
@Temperature 30.0 - 700 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
 0.485 J/g-°C
@Temperature 100 °C
 0.515 J/g-°C
@Temperature 200 °C
 0.545 J/g-°C
@Temperature 300 °C
 0.570 J/g-°C
@Temperature 400 °C
 0.590 J/g-°C
@Temperature 500 °C
 0.605 J/g-°C
@Temperature 600 °C
 0.615 J/g-°C
@Temperature 700 °C
Thermal Conductivity 12.0 W/m-K
@Temperature 20.0 °C
 14.0 W/m-K
@Temperature 100 °C
 16.0 W/m-K
@Temperature 200 °C
 18.0 W/m-K
@Temperature 300 °C
 20.0 W/m-K
@Temperature 400 °C
 22.0 W/m-K
@Temperature 500 °C
 23.0 W/m-K
@Temperature 600 °C
 25.0 W/m-K
@Temperature 700 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 20 %
Copper, Cu 1.5 %
Manganese, Mn 1.8 %
Molybdenum, Mo 4.5 %
Nickel, Ni 25 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.50 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® 954-3 Curing Cyanate Resin, K13C-2U Fiber
Overview of materials for Solder/Braze Alloy
Overview of materials for Epoxy/Carbon Fiber Composite
Overview of materials for Copper Alloy

NSANDV5150 / 199714

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.