MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PTS Trimid® N66-G13HL 13% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 117.2 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Modulus 4.69 GPaASTM D790
Izod Impact, Notched 0.480 J/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 254 °CASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 243 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 490 °F
Middle Barrel Temperature 515 °F
Front Barrel Temperature 545 °F
Nozzle Temperature 510 - 540 °F
Melt Temperature 520 - 560 °F
Mold Temperature 80.0 - 200 °F
Drying Temperature 160 °F
Dry Time 4 hour
Injection Pressure 10000 psi
Back Pressure 10.0 - 100 psi
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
PTS Trimid® N66-G43HL 43% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
PTS Trimid® N66-G13L 13% Glass Fiber Reinforced Lubed Nylon 6/6
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled

PZ9PT46 / 21495

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.