The LW/CS/UV Series is a lightweight material solution for applications with superior requirements on sealing performance. The compounds are especially suited for automotive exterior applications. They are available in black colors. Processing Method: Injection Molding, Extrusion Color / RAL DESIGN: Typical applications: - Automotive Exterior
- Seals
- Cowls gaskets
- Glass Run Channel
- Door sills
- Seals for windows and doors
- Grommets
- Heavy-walled parts
Material advantages:- Low density
- Adhesion to PP
- Optimized compression set
- UV and weathering resistance
- Resilience
- Non-sticky surface
- In-process recycling possible
Information provided by Kraiburg TPE |