MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Quaker Quintolubric® 814-02 Longwall Roof Support
Categories: Fluid

Material Notes: Benefits:
  • Approved by Joy Mining Machinery at 2% concentration in two classes of water: <125 ppm CaCO3 and Type 18 water
  • Approved by Caterpillar in mine specific water
  • Approved by MSHA - No. 30-20-5
  • Biodegradable in accordance with ISO 7827
  • Compatible with all commonly used longwall fluids for easy conversion
  • Optional dye for easy underground leak detection
Applications: QUINTOLUBRIC® 814-02 is a high water-based (HFA) hydraulic fluid concentrate designed for use in longwall shields.

Information provided by Quaker

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccASTM D287
pH 10.12% Distilled Water; ASTM D70
Viscosity Measure 108 cSt
@Temperature 37.8 °C
ASTM D445
Storage Temperature 0.000 - 43.3 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point -4.40 °CFreezing Point; ASTM D97
 
Descriptive Properties
AppearanceTranslucent Amber Green Solution
Recommended Concentration0.02

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WQUAK004 / 184990

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.