Lewatit® S 100 KR-H Cl-frei is a strongly acidic, gel-type cation exchange resin in highly regenerated form (min. 99% H) and purified (extremely low content of desorbable chloride ions) to meet nuclear industry specifications. Lewatit nuclear resins (Lewatit KR) are noted for their outstanding mechanical, osmotic and chemical stability. Used in radioactive water circuits, they provide a number of special tasks and guarantee a water quality that fully complies with the requirements of the nuclear power industry. Lewatit® S 100 KR-H Cl-frei is particularly suitable for:- the removal of cations, including radioactive isotopes, from aqueous solutions (pH control through adsorption of excess Li)
- the decontamination of circuits in nuclear reactor plants
- the removal of radioactive cations such as cesium 137 (fuel cooling)
- the treatment of primary coolant e.g. in pressure water reactors
- the removal of activated cleavage or corrosion products, including mechanical filtration of suspended impurities
- the polishing in the primary and secondary sections as a mixed bed component with Lewatit MonoPlus M 500 KR or Lewatit MonoPlus M 800 KR.
Important! Rinse carefully with demineralized water prior to service or mixing with Lewatit MonoPlus M 500 KR or Lewatit MonoPlus M 800 KRInformation provided by Lanxess. |