Standard Applications: RHODOLINE® 4100 is a very effective APE free anionic wetting and dispersing agent in both water and solvent based industrial systems. RHODOLINE® 4100 exhibits improved film properties including gloss, color acceptance and adhesion. Recommended usage levels typically are 0.1 – 0.5% active as wetting agents for paint formulations, 1 – 2% active for pigment wetting and 5 – 20% active on the pigment weight for pigment dispersing. Chemical Name: Anionic Wetting and Dispersing Agent Information provided by Solvay |