MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain COHRlastic® CF4420 High Heat Reinforced Solid Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six constructions. CF 4420 is specially formulated for thermal stability and long life under extreme heat and pressure for extended dwell times. It resists reversion (i.e. softening and outgassing) longer than general purpose silicone. Throughout its useful life, 4420 has thermal stability for consistent thermal conductivity. All data based on a 0.0625 inch test sample.(Also available in 0.045"; Thickness shown is for silicone rubber. Fiberglass thickness = 0.014".)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content <= 0.50 g/lWeight Loss (4 hrs at 400°F)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
Elongation at Break <= 10 %
Flexural Strength 500 psiDiaphragm Burst Strength
Tear Strength 300 pli
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 500 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µin/in-°F
@Temperature 20.0 °C
Silicone rubber component
Thermal Conductivity 1.90 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain COHRlastic® CF4480 High Heat Reversion Resistant Reinforced Solid Rubber
Saint-Gobain COHRlastic® 100S Silicone Sponge/High Temp Silicone Adhesive Pressure Sensitive Tape

PSTGQZ248 / 68762

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.