MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC SABIC® PP QR678K PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PP QR678K is a very high melt flow index random copolymer with high transparency and good antistatic properties. This grade combines improved aesthetics of the finished articles with low temperature processability. Part aesthetics are not affected by the lower processing temperatures, providing for a broader operating window. The SABIC® PP QR678K presents very high melt flow rate, easy demoulding and good stiffness to impact ratio. Application: SABIC® PP QR678K is mainly used in injection moulding processes. The SABIC® PP QR678K is typically used at transparent applications were higher MFI’s with good flow are required. Its intended applications include injection moulded housewares, office & home storage boxes, thin wall packaging and media packaging. The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/medical applications. IMDS 80775790

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64ISO 868
Tensile Strength, Yield 28.0 MPaSpeed of testing: 50 mm/min; ISO 527-2 1A
Elongation at Yield 13 %ISO 527-2 1A
Tensile Modulus 1100 MPaSpeed of testing: 1 mm/min; ISO 527-2 1A
Izod Impact, Notched (ISO) 3.50 kJ/m²ISO 180/1A
 1.50 kJ/m²
@Temperature 0.000 °C
ISO 180/1A
Charpy Impact, Notched 1.50 kJ/m²ISO 179/1eA
 4.00 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °CFlat wise ( testbar 80*10*4mm); ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CFlat wise ( testbar 80*10*4mm); ISO 75
Vicat Softening Point 70.0 °Cat 50 N (VST/B); Temperature rate: 120°C/h; ISO 306
 125 °Cat 10 N (VST/A); Temperature rate: 120°C/h; ISO 306
 
Descriptive Properties
Anti static agentTrue
ClarifiedTrue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11264 / 244731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.