System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Celanese Zytel® 70G25HSLR BK099 PA66-GF25
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 30% Glass Fiber Filled
Material Notes:
25% Glass Reinforced, Heat Stabilized, Hydrolysis Resistant, Polyamide 66
Former DuPont product acquired by Celanese in 2022.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.32
g/cc
DAM; ISO 1183
Water Absorption
1.4 %
@Time 86400 sec
Immersion; DAM; Sim. to ISO 62
Viscosity Number
150
cm³/g
DAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow
0.0030
cm/cm
DAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.011
cm/cm
DAM; ISO 294-4, 2577
Melt Flow
25
g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
120
MPa
50% RH; ISO 527-1/-2
180
MPa
DAM; ISO 527-1/-2
Elongation at Break
3.0 %
DAM; ISO 527-1/-2
6.0 %
50% RH; ISO 527-1/-2
Tensile Modulus
6000
MPa
50% RH; ISO 527-1/-2
8500
MPa
DAM; ISO 527-1/-2
Flexural Strength
170
MPa
50% RH; ISO 178
260
MPa
DAM; ISO 178
Flexural Modulus
5500
MPa
50% RH; ISO 178
8000
MPa
DAM; ISO 178
Poissons Ratio
0.34
DAM
0.35
50% RH
Izod Impact, Notched (ISO)
7.00
kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
7.00
kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
10.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO)
50.0
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1U
50.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1U
50.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
80.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1U
Charpy Impact Unnotched
60.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
60.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
80.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched
10.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
11.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Electrical Properties
Original Value
Comments
Dielectric Strength
24.0
kV/mm
@Thickness 1.00 mm
Short Time; DAM; IEC 60243-1
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
29.0
µm/m-°C
DAM; ISO 11359-1/-2
18.0
µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
34.0
µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow
88.0
µm/m-°C
DAM; ISO 11359-1/-2
76.0
µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
130
µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Melting Point
262
°C
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
261
°C
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
252
°C
DAM; ISO 75-1/-2
Flammability, UL94
HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
HB
@Thickness 3.00 mm
DAM; IEC 60695-11-10
Flame Spread
27.0
mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Processing Properties
Original Value
Comments
Melt Temperature
295
°C
Optimum, Injection
285
-
305
°C
Range, Injection
Mold Temperature
70.0
-
120
°C
Injection
100
°C
Optimum, Injection
Ejection Temperature
210
°C
Injection
Drying Temperature
80.0
°C
Injection
Dry Time
2.00
-
4.00
hour
Injection, Dehumidified Dryer
Moisture Content
<= 0.20 %
Injection
Hold Pressure
50.0
-
100
MPa
Range, Injection
Descriptive Properties
Additives
Release agent
Drying Recommended
yes
Injection
FMVSS Class
B
ISO 3795 (FMVSS 302)
ISO designation
ISO 16396-PA66,GF25,M1CGHRW,S14-080
Max. screw tangential speed (m/s)
0.2
Injection
Part Marking Code
>PA66-GF25<
ISO 11469
Polymer
PA66-GF25
Processing Hold Pressure Time (s/mm)
3
Injection
Resin Identification
PA66-GF25
ISO 1043
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 70G25HSL NC010 PA66-GF25
Celanese Zytel® 70G25HSLR NC010 PA66-GF25
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25
EMS-Grivory Grilon® AG-25 HM PA66-GF25
DuPont Mobility and Materials Zytel® 70G30HSL BK039B PA66-GF30
PDSX5321 / 197961
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.