MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Easy-flo™ High Temperature Grade Flux Paste Brazing Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Easy-flo™ High Temperature Flux Paste a brazing flux suitable for use with silver brazing filler metals. It has a working range of 575-825°C and can be used with silver brazing filler metals melting below 775°C. Easy-flo™ High Temperature Flux Paste formerly sold as Easy-flo™ Flux Paste.

Easy-flo™ High Temperature Flux Paste exhibits better life at temperature and greater overheat resistance than many other flux pastes. Easy-flo™ High Temperature Flux paste has a low melt viscosity and as such performs well when pasted onto vertical surfaces, and can be useful when brazing stainless steel. The molten viscosity of Easy-flo™ High Temperature Flux Paste is such that it holds on vertical surfaces. It is therefore particularly useful when brazing joints in positions where other fluxes may have a tendency to run away from the joint.

It is suitable for use on all the common engineering materials, (copper, brass, mild steel and stainless steel), but not aluminum. JM special purpose fluxes are required when brazing aluminum bronze, certain grades of stainless steel, tungsten, molybdenum and tungsten carbide or where protracted heating is involved.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 575 - 825 °C
Solidus 575 °C
Liquidus 825 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey Silver-flo™ 55 Cadmium Free Silver Brazing Filler Metal

NJMMJ9731 / 186132

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.