MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay ALKAMULS® PSML 20 Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Sorbitan ester ethoxylate with a HLB of 16.7. Oil in water emulsifier for mineral and vegetable oils in metalworking. Solubilizer, antistat and lubricant for textile industry.

Chemical Name: ETHOXYLATE SORBITAN MONOLAURATE

CAS: 68154-33-6; 7732-18-5

Soubility: Mineral Oil-Insoluble; Aromatic-Soluble; Aliphatic-insoluble

Available in: Asia Pacific, Europe, Latin America and North America

Applications: ALKAMULS ® PSML-20 is a polyethoxylated sorbitan monolaurate with approximately 20 moles of ethylene oxide. Emulsifier and co-emulsifier for petroleum oils, fats, solvents and waxes in cosmetics. Viscosity modifier in non-irritating shampoos. Co-emulsifier in dye carrier formulations. Spin aid for nylon and fines aid for rayon finishing. Low order of toxicity. Good emulsification characteristics, particularly in combination with high or low HLB surfactants to form W/O or O/W emulsions. Bath Product, Body Wash, Cream and Body Lotion, Deodorant, Facial Cream, Facial Cleanser, Fragrance, Liquid Soap, Shampoo, Suncare Products

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 2.0<= 2.0[mg KOH/g]; RP-0008
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 149 °C>= 300 °FCOC; ASTM D92
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 3.0 %<= 3.0 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClean, Clear LiquidRP-0064
HLB number16.7
Hydroxyl Number96-108 mg KOH/gRP-0245
Saponification number40-50 mg KOH/gRP-0496

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay ALKAMULS® PSMO 20 Surfactant
Solvay ALKAMULS® EL 620 Surfactant

WRHOD048 / 137278

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.