MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Vistamaxx™ 6102FL Propylene-based Elastomer - Performance Film
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO), Film Grade

Material Notes: Product Description: Vistamaxx 6102FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. The "FL" designates this product passes ExxonMobil Chemical's test for film appearance with regard to gels, as needed for performance film applications ('A' rating).

Key Features:

  • Suitable for a wide range of cast and blown film applications, and melt-spun nonwoven applications.
  • Very good elasticity.
  • Can be blended with PE, PP and other polymers, including styrenic block copolymers.
  • Excellent adhesion to conventional and metallocene PP and PE.
  • Good cling and tack in stretch film and protective film applications.
  • Good sealing properties.
  • Good chemical resistance to aqueous systems and non-hydrocarbon based fluids.
  • May be used in food contact applications (with some restrictions).
  • EU and China RoHS compliant.
Applications:
  • Blown Film
  • Cast Film
Uses:
  • Compounding
  • Film
  • Packaging
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.862 g/ccASTM D1505
Melt Flow 3.0 g/10 minmelt flow rate; ExxonMobil Method
 1.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 66
@Time 15.0 sec
ASTM D2240
Tensile Stress at Strain 1.90 MPa
@Strain 100 %
ASTM D412
 2.20 MPa
@Strain 300 %
ASTM D412
Flexural Modulus, 1% Secant 12.3 MPaASTM D790
Tear Strength 34.4 kN/mDie C; ASTM D624
Tensile Set 18 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 52.2 °CASTM D1525
 
Descriptive Properties
Ethylene Content16.0 wt%ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer
ExxonMobil Vistamaxx™ 6102 Propylene-based Elastomer
ExxonMobil Vistamaxx™ 3020FL Propylene-based Elastomer - High Purity, Low Gel
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel

PEXA939 / 125982

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.