Moplen RP325M is a controlled rheology medium modified polypropylene random copolymer. It contains slip and anti-blocking additives. Moplen RP325M is typically used for manufacturing of un-oriented cast films. Customer report lamination, textile and packaging of foodstuffs as typical applications. Moplen RP325M exhibits good processability, and that films produced with Moplen RP325M exhibits high clarity and gloss, softness and good heat weldability. Applications: Food Packaging Film, Lamination Film, Stationery Film, Textile Packaging Film.Information provided by LyondellBasell. |