MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior No. 119SFM Bromide-Based Radiator Core Baking Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Bromide-Based Flux for Copper-Brass Radiator Core Baking
  • Excellent Radiator Soldered Tube to Radiator Copper Fin Bonding
  • Highly Concentrated Formulation to Permit Great Dilution
  • Does Not Turn Radiator Cores Green After Core Baking
Description: Superior No. 119SFM is a concentrated, zinc-free, organic hydrobromide type formulation with excellent wetting and fluxing action. Superior No. 119SFM leaves no residue after core baking that requires removal and its unique chemistry eliminates the possibility that parts will turn green after soldering.

Applications: Superior No. 119SFM is intended for use in copper/brass radiator core fusing operations using a continuous type baking oven. This formulation has been optimized for good core bonding with a high flux dilution ratio. Normal flux application procedures can be used, with dip immersion or spraying generally recommended. Superior No. 119SFM is normally applied at room temperature.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.112 - 1.132 g/cc1.112 - 1.132 g/cc
Density 1.12 g/cc0.0405 lb/in³
Surface Tension 32 dynes/cm32 dynes/cm
 
Processing PropertiesMetricEnglishComments
Processing Temperature 400 - 750 °C752 - 1380 °FSoldering Range
 
Descriptive Properties
FormClear, Colorless to Yellow
Free Acid1.85-2.85%HBr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSFLUX043 / 185727

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.