MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond Supreme 121AOND Two part toughened epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Paste consistency
  • High temperature resistance
  • Exceptionally long open time
  • Passes NASA low outgassing
Product Description: Master Bond Supreme 121AOND is a thermally conductive epoxy for bonding, sealing and encapsulation. The mix ratio is 100:80 by weight. This system has a very long open time of 2-3 days and after mixing, it is a paste. Supreme 121AOND requires oven curing. A typical cure schedule would be 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will further enhance product properties. Supreme 121AOND combines a high glass transition temperature along with an element of toughness, making it less rigid than typical higher temperature resistant epoxies. Supreme 121AOND bonds to a wide variety of substrates including metals, composites, glass, and many rubbers and plastics. It adheres especially well to glass, fibers and ceramics. This system can withstand thermal cycling and mechanical stresses. Its physical strength profile is strong and steadfast, particularly its tensile modulus. It is a reliable thermal conductor while retaining excellent insulation properties. Supreme 121AOND has good resistance to chemicals including water, oils, fuels, acids and bases. The color of Part A is black and Part B is dark brown. Its service temperature range is -80°F to +550°F. It should be noted that Supreme 121AOND is particularly well suited for bonding and sealing applications. It should be considered in demanding aerospace, electronic, opto-electronic and specialty OEM type applications where this product profile is needed.

Product Advantages:

  • Paste consistency with a long working life
  • Thermally conductive, electrically insulative
  • Superior physical strength properties
  • High glass transition temperature
  • Has an element of toughness
  • Combines exceptionally low shrinkage and high dimensional stability

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 5000 - 15000 cP5000 - 15000 cPPart A
 10000 - 25000 cP10000 - 25000 cPMixed
 50000 - 300000 cP50000 - 300000 cPPart B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85 - 9585 - 95
Tensile Strength 41.4 - 48.3 MPa6000 - 7000 psi
Tensile Modulus  4.48 - 5.17 GPa
@Temperature 149 °C
650 - 750 ksi
@Temperature 300 °F
 5.17 - 5.86 GPa
@Temperature 23.9 °C
750 - 850 ksi
@Temperature 75.0 °F
Compressive Strength 179 - 193 MPa26000 - 28000 psi
Adhesive Bond Strength 16.5 - 17.9 MPa2400 - 2600 psiTensile lap shear
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cm
 >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.576 - 0.720 W/m-K4.00 - 5.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C550 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
Glass Transition Temp, Tg 200 - 210 °C392 - 410 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 93.3 - 98.9 °C
1.00 - 2.00 hour
@Temperature 200 - 210 °F
Step 1
 120 - 240 min
@Temperature 177 °C
2.00 - 4.00 hour
@Temperature 350 °F
Recommended post cure to enhance properties
 180 - 240 min
@Temperature 121 °C
3.00 - 4.00 hour
@Temperature 250 °F
Step 2
 240 - 360 min
@Temperature 149 °C
4.00 - 6.00 hour
@Temperature 300 °F
Step 3
Working Life 48.0 - 72.0 min48.0 - 72.0 minafter mixing, 100 gram batch
Shelf Life 6.00 Month6.00 Monthin original, unopened containers
 
Descriptive Properties
Mixing ratio100:80 by weightParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5943 / 306832

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.