MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow UNIVAL™ DMDC-6400 NT 7 High Density Polyethylene Resin (HDPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes:
  • Excellent process-ability
  • Moderate swell
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2
UNIVAL™ DMDC-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, water and fruit drinks. In addition, it can be blow molded into other thin-walled parts and houseware items, and also can be extruded into sheets and profiles.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.961 g/ccASTM D792
ESCR 100% Igepal® 20 hour
@Temperature 50.0 °C
F50; Molded and tested in accordance with ASTM D4976; ASTM D1693
High Load Melt Index 47 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Melt Index of Compound 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 4200 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 4300 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 1000 %Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 7.0 %Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 180000 psi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength 60.0 ft-lb/in²Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
 
Thermal PropertiesOriginal ValueComments
Melting Point 273 °FDow Method (DSC)
Crystallization Temperature 120 °CDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 174 °FMolded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point 266 °FASTM D1525
Brittleness Temperature <= -105 °FMolded and tested in accordance with ASTM D4976; ASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DMDA-8907 NT 7 High Density Polyethylene Resin
Dow UNIVAL™ DMDH-6400 NT 7 High Density Polyethylene Resin (HDPE)
Dow HDPE 30460M High Density Polyethylene
Dow UNIVAL™ DMDD-6200 NT 7 High Density Polyethylene Resin (HDPE)
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)

PDOW1464 / 30682

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.