MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Baydur® TB 100-15 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: The Baydur TB 100-15 thermal break system produces a structural, full density polyurethane used for window applications.

Properties / Applications: The Baydur TB 100 15 thermal break system produces a structural, full density polyurethane used for window applications. The system is supplied as two reactive liquid components. Component A is a polymeric diphenylmethane diisocyanate (PMDI), and Component B is a formulated polyol system that is phase stable. Baydur TB 100-15 is a fast debridging system, designed to have excellent physical properties while exhibiting minimal wet shrinkage. As with any product, use of the Baydur TB 100-15 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccPolyol (Component B)
 1.15 g/ccASTM D1622
 1.24 g/ccIsocyanate (Component A)
Viscosity 200 cPIsocyanate (Component A)
 600 cPPolyol (Component B)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78
@Time 5.00 sec
ASTM D2240
Tensile Strength at Break 39.3 MPaASTM D638
Elongation at Break 30 %ASTM D638
Flexural Modulus 1550 MPaASTM D790
Izod Impact, Notched 1.90 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.900 BTU-in/hr-ft²-°FASTM C518
Deflection Temperature at 0.46 MPa (66 psi) 81.1 °CASTM D648
 
Descriptive Properties
AppearanceBlack liquidPolyol (Component B)
 Dark brown liquidIsocyanate (Component A)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baydur® 742 IBS Polyurethane Structural Foam RIM, Density 43 pcf
BCC Products MB 1100 Polyurethane Foam Modeling Board
BCC Products Kwik Kast BC 8001 Urethane Casting
BCC Products BC 8660E Urethane Elastomer
BASF Elastollan® S 74 D TPUR

PCOVEST0105 / 201888

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.