MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cyclewood Solutions Xylomer™ XM1-GQD Compostable Film Resin
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic

Material Notes: 100% biodegradable and compostable thermoplastic. The compostable resin blend performs well compared to LDPE and is BPI certified compostable under ASTM D-6400. Xylomer™ is modified lignin, an abundant, natural byproduct of the paper manufacturing process, blended with other compostable polymers. The main benefit of using Xylomer™ technology is that Xylobag™ bags break down into humus in approximately 180 days once it has reached the natural environment, improving soil structure and leaving a cleaner environment. With government regulation restricting the use of harmful high-density polyethylene bags, the Xylobag™ provides retailers with a viable, cheap bag alternative. The Xylobag™ allows consumers to eliminate unsightly plastic litter from their communities.

Information provided by Cyclewood Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/cc
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 263 %
Film Elongation at Break, TD 382 %
Elmendorf Tear Strength MD 204 g
Elmendorf Tear Strength TD 706 g
Dart Drop Test 118 g
Film Tensile Strength at Break, MD 2083 psi
Film Tensile Strength at Break, TD 1574 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BiologiQ ESR-PE EcoStarch mLLDPE Blend
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic
SK Chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic
SK Chemicals SKYTHANE® SG100 SKYGREEN Biodegradable Thermoplastic

PCYCLEW95 / 177971

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.