MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMODURE® N 3368A BA/SN Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Desmodur N 3368A BA/SN is an aliphatic polyisocyanate (HDI trimer). It is suitable as the hardener component for lightfast polyurethane coating systems.

Properties / Applications: Desmodur N 3368A BA/SN is used primarily as the hardener component for lightfast two-component polyurethane coatings with high resistance to chemicals and weathering, very good gloss retention and outstanding mechanical properties. Preferred co-reactants are polyacrylate or polyester polyols. The main applications for systems based on Desmodur N 3368A BA/SN are air- and force-drying coatings for automotive OEM, automotive refinishing, transportation, industrial finishing and plastics. As with any product, use of Desmodur N 3368A BA/SN in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Volatiles 31 - 33 %2.2 g / 120 min / 100°C
Viscosity 30 - 60 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point 37.0 °C
 
Descriptive Properties
Color<40Hazen
Content<0.15Monomeric HDI
 14.5-15.1%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODURE® N 3390A BA/SN Polyurethane
Covestro DESMODURE® PL 340 BA/SN Polyurethane
Covestro DESMODURE® PL 350 MPA/SN Polyurethane
Covestro Desmodur® XP 2619 Polyurethane
Covestro DESMODURE® N 100A Polyurethane

PCOVEST0558 / 202341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.