MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lehvoss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer with PTFE, lubricant modified
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, PTFE Filled

Material Notes: Properties/attributes include: Improved friction and wear behavior. Emergency (dry) running property. Sliding-couples with a low friction coefficient. High dimensionally stable precision parts.

Automotive industry, textile- and office machinery, apparatus- and precision engineering. Typical uses include: Bearings, sleeves, high precision gear wheels, control disks, rollers, coil formers.

Processing: If originally sealed containers are used, it is normally possible to omit the predrying stage. If PTFE materials are not predried, an increase in deposits inside the mould may occur. When changing from higher melting-point polymers such as polyamides to this product, extremely thorough intermediate cleaning should be carried out. Processing temperatures above 215°C may very rapidly cause thermal damage and should therefore be avoided, particularly as formaldehyde may be eliminated here. Therefore, ventilation of machinery is recommended. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccISO 1183
Moisture Absorption <= 0.100 %
@Temperature 23.0 °C,
Time 86400 sec
Linear Mold Shrinkage 0.018 - 0.025 cm/cmDIN 16901
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 40.0 MPaISO 527-2
Elongation at Break 15 %ISO 527-2
Modulus of Elasticity 2.00 GPaISO 527-2
Flexural Strength 60.0 MPaISO 178
Flexural Modulus 1.80 GPaISO 178
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1fu
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179 eA
 12.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+12 ohm-cmIEC 60167
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CDIN 53752
Thermal Conductivity 0.200 W/m-KDIN 52612
Maximum Service Temperature, Air 100 °CContinuous; UL 746B
 120 °CShort Term
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CISO 75-2/A
Vicat Softening Point 160 °CVST A; DIN ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 175 - 200 °C
Zone 1 175 - 190 °C
Zone 2 185 - 205 °C
Zone 3 180 - 200 °C
Melt Temperature 200 °C
Mold Temperature 80.0 - 120 °C
Drying Temperature 75.0 °C
@Time 7200 - 28800 sec
Dehumidifying dryer
 120 °C
@Time 7200 - 14400 sec
Air-Circulation Dryer
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 80/TF/22/NT Polyacetal-copolymer with PTFE
Lehvoss LUVOCOM® 80/CF/12/TF/10/BK 100 Polyacetal-copolymer with carbon fiber and PTFE
Westlake Plastics Dielux® PTFE filled Acetal Copolymer
LATI Latilub 73/13-10T Y/15 POM, 15% Aramid Fiber Reinforced, PTFE Filled
Kolon KOCETAL® TF304 Wear Modified Acetal Resin

PLUU8927 / 193886

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.