MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta RM629 Rolled and Molded Rod, Cotton Fabric with Phenolic Resin Systemm, NEMA XX
Categories: Polymer; Thermoset; Phenolic

Material Notes: Rolled and Molded Rods are made from an alpha paper impregnated with an electrical grade of phenolic resin. RM629 is used for electrical and mechanical applications, meeting ANSI/NEMA IM 60000-2021 Grade XX, MIL-I-24768/11 PBG and ASTM D709 Type I Grade XX requirements.

Information provided by Norplex Micarta.

Key Words: Cotton Fiber, Phenolic, ANSI/NEMA IM 60000-2021 Grade XX, MIL-I-24768/11 PBG and ASTM D709 Type I Grade XX
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100
Tensile Strength 15300 psiCondition A
Flexural Strength 20800 psiCondition A
Compressive Strength 27900 psiCondition A
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 140 °C
UL RTI, Mechanical with Impact 140 °C
Flammability, UL94 HBCondition A
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.580 %Condition D; ASTM D-349
 
Descriptive Properties
Rod Diameter0.5 inch (1.3 mm)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNORPM915 / 323352

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.