MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hytrel® 5556 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 55 Shore D High Performance Polyester Elastomer

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Melt Density 1.03 g/cc
@Temperature 230 °C
Water Absorption 0.60 %
@Time 86400 sec
Immersion; Sim. to ISO 62
 0.60 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
Sim. to ISO 62
Water Vapor Transmission 300 g/m²/day23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission 6000 cc-mm/m²-24hr-atm23°C/85%r.h.; DIS 15105-1/-2
Thickness 25.0 micronsAs Tested
Linear Mold Shrinkage, Flow 0.014 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cmISO 294-4, 2577
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 220 °C
cm³/10min Volumetric; ISO 1133
 7.8 g/10 min
@Load 2.16 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 2400 N
@Temperature 23.0 °C
maximum force; ISO 6603-2
 3700 N
@Temperature -30.0 °C
maximum force; ISO 6603-2
Hardness, Shore D 5115s; ISO 48-4
 <= 55ISO 48-4
Tensile Stress at Strain 6.90 MPa
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 11.0 MPa
@Strain 10 %
ISO 527-1/-2
 14.5 MPa
@Strain 50 %
ISO 527-1/-2
 16.0 MPa
@Strain 100 %
ISO 527-1/-2
Tensile Modulus 180 MPaISO 527-1/-2
Flexural Modulus 190 MPaISO 178
Poissons Ratio 0.48
Izod Impact, Notched (ISO) NB
@Temperature -40.0 °C
ISO 180/1A
 NB
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 145 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 145 kJ/m²
@Temperature -30.0 °C
Partial Break; ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
Tensile Impact Strength 320 kJ/m²
@Temperature 23.0 °C
Notched; ISO 8256/1
Puncture Energy 27.0 J
@Temperature 23.0 °C
ISO 6603-2
 43.0 J
@Temperature -30.0 °C
ISO 6603-2
Tensile Creep Modulus, 1 hour 170 MPa1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 133 MPa1000h; ISO 899-1
Tear Strength 134 kN/mnormal; ISO 34-1
 137 kN/mparallel; ISO 34-1
Abrasion 120mm3; ISO 4649
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+15 ohmIEC 62631-3-2
Dielectric Constant 4.4
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.8
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 19.0 kV/mmIEC 60243-1
Dissipation Factor 0.0090
@Frequency 100 Hz
IEC 62631-2-1
 0.0375
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 180 µm/m-°CISO 11359-1/-2
 160 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°CISO 11359-1/-2
 174 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
Specific Heat Capacity 2.11 J/g-°C
@Temperature 230 °C
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature 230 °C
Melt
Melting Point 201 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1/-2
Vicat Softening Point 75.0 °C50°C/h, 50N; ISO 306
 180 °C50°C/h 10N; ISO 306
Brittleness Temperature -98.0 °CISO 974
Glass Transition Temp, Tg -25.0 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 HB
@Thickness 3.00 mm
IEC 60695-11-10
Oxygen Index 20 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 225 °COptimum, Extrusion
 220 - 235 °CRange, Extrusion
 230 °COptimum, Injection
 220 - 250 °CRange, Injection
Mold Temperature 45.0 °COptimum, Injection
 45.0 - 55.0 °CInjection
Drying Temperature 100 °CInjection
 90.0 - 110 °CExtrusion
Dry Time 2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 <= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)7E-08
Emission of organic compounds (µgC/g)8.5VDA 277
FMVSS ClassSEISO 3795 (FMVSS 302)
Fogging (mg)0.1G-value (condensate); ISO 6452
Light stability delta a-2DIN 53236
Light stability delta b13DIN 53236
Light stability delta E14DIN 53236
Light stability delta l3DIN 53236
Odor Class5VDA 270
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® 6356 TPC-ET
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer
Celanese Hytrel® 4056 TPC-ET
Celanese Hytrel® 4068 TPC-ET
Celanese Hytrel® 4069 TPC-ET

PDSX5185 / 197825

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.