MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TIMCAL C-NERGY™ KS 6L Graphite
Categories: Carbon; Carbon Black; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Characteristics:
  • The total Fe content for our conductive carbon blacks is less than 5 ppm
  • The total Fe content for our graphite is less than 20 ppm
  • C-NERGY grades have very low total metallic impurity content
  • The BET surface area for our conductive carbon blacks is lower than competition
  • Our graphite has well-defined particle size distribution (PSD)
  • Well-suited for lithium-ion battery processing environment
  • Our conductive carbon blacks have high structure, which can be seen from the high oil absorption number (OAN)
  • Our graphite has high crystallinity
  • Low dosage is sufficient to achieve the percolation threshold
  • Compressibility can be increased with the addition of fine graphite particles having high crystallinity and low spring back
Application Benefits:
  • Increased battery safety
  • Lower rejection ratio
  • Fully compatible with most electrolyte systems
  • No additional pre-dispersing unit is needed
  • No dispersing aid is needed
  • Very high loading is possible
  • Cost savings on NMP and faster drying time when C-NERGY SUPER C45 is applied
  • High energy density
  • Improved power density
  • Cost reduction thanks to lower dosage needed
  • High energy density
  • Improved power density
  • Improved “flexibility” of the electrode

Information provided by TIMCAL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Surface Area 20 m²/gBET
Ash 0.010 %
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMCAL C-NERGY™ SUPER C65 Carbon Black Additive
TIMCAL SUPER P® Li Carbon Black Additive
Graphite, Carbon, C
Cancarb Thermax® Powder N991 Medium Thermal Carbon Black
TIMCAL TIMREX® SFG6 Primary Synthetic Graphite

CTIMCAL907 / 140866

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.