MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxies, Etc 10-3005 NS Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: These high bond strength adhesives are clear 100% solids, two component, non-sag adhesives with a quick setting time of 5-46 minutes at room temperature. They are excellent for bonding plated metals, pewter, glass, wood, ceramic, felt, cement, gem stones, most plastics and rubbers, etc. These adhesives were tested in our laboratory for flame retardancy properties. According to our test results they meet the requirements of UL94HB.

Applications: These unique adhesives are ideally suited for a wide range of electronic, electrical, industrial, structural, and jewelry applications. These adhesives are also an excellent choice for field repairs. They are offered in the popular TriggerBond® dual barrel cartridge dispensing system and bulk packaging.

Features:

  • Non-sag consistency
  • High bond strength
  • Fast room temperature cure – three speeds to choose from
  • Water & chemical resistance
  • Outstanding thermal shock resistance
  • 1:1 mix ratio
  • Impact resistance

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Compressive Modulus 0.0586 GPa8.50 ksi
Shear Strength 1.72 MPa250 psiPolycarbonate
 2.31 MPa335 psiPVC
 3.45 MPa500 psiABS
 5.00 MPa725 psiBrass
 5.17 MPa750 psiStainless Steel
 6.21 MPa900 psiGalvanized Steel
 6.62 MPa960 psiCopper
 6.89 MPa1000 psiCold rolled steel
 10.3 MPa1500 psiAluminum (etched)
Izod Impact, Notched 1.44 J/cm2.70 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm
Dielectric Constant 4.0
@Frequency 1000 Hz
4.0
@Frequency 1000 Hz
Dielectric Strength 16.5 kV/mm420 kV/in
Dissipation Factor 0.017
@Frequency 1000 Hz
0.017
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C33.3 µin/in-°F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 - 20.0 min0.250 - 0.333 hour
 1440 - 2880 min24.0 - 48.0 hourHandling time
 
Descriptive Properties
ColorSemi-transparent (available in black)
Mix Ratio1:1by volume
Working Time3-5 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX074 / 316751

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.