MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Entec Hylex® P1017FR Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes:

Information provided by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 17 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8700 psiASTM D638
Elongation at Break 110 %ASTM D638
Flexural Strength 14000 psiASTM D790
Flexural Modulus 360000 psiASTM D790
Izod Impact, Notched 10.0 ft-lb/in73°F, 0.125 in; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 285 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 265 °FUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.57 mm
NA
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 470 - 510 °F
Middle Barrel Temperature 490 - 520 °F
Front Barrel Temperature 520 - 540 °F
Nozzle Temperature 510 - 530 °F
Melt Temperature 520 - 550 °F
Mold Temperature 160 - 200 °F
Drying Temperature 250 °F
Dry Time 3 - 12 hour
Moisture Content <= 0.020 %
Injection Pressure 900 - 1800 psi
Back Pressure 70.0 - 150 psi
Shot Size 40 - 60 %
Screw Speed 40 - 70 rpm
 
Descriptive Properties
Holding Pressure600 to 1100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylex P1010FRMAUV Polycarbonate
Ravago Manufacturing Americas Hylex P1317L Polycarbonate
Ravago Manufacturing Americas Hylex P1010G7FRMA Polycarbonate
Mitsubishi Lemalloy® BX505 PPE-PA6 Alloy
Lotte Advanced Materials Infino® LH-1070W PC, FR

PENTA046 / 36065

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.