MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Maxxam™ FR PP 853 Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Melt Flow 0.91 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Procedure A; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2.07 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 300 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 1380 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 31.7 MPaASTM D790
Flexural Modulus 1240 MPaASTM D790
Izod Impact, Notched 320 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Gardner Impact 21.5 J
@Thickness 3.18 mm,
Temperature 23.0 °C
ASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 3.00 mm
All colors; UL 94
Oxygen Index 26 %
@Thickness 3.18 mm
ASTM D2863
 
Descriptive Properties
FeaturesFlame Retardant
 Low Flow
FormsPellets
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 199 X 138286 Polypropylene (PP); Flame Retardant - Halogen Free - Glass Fiber - Mineral - Chemically Coupled
Loxim 830 01 HB Polypropylene Compound, Flame Retardant
LG Chemical LUPOL GP1000FC Flame Retardant PP
Addiplast Addilene PMD 50265 Flame Retardant Polypropylene

PH1PN9139 / 102975

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.