MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Traid Villarroya TKG® 500 PE-HMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes:
  • Very low water absorption
  • Resistant to dilute acids, solvents and cleaning agents
  • UV resistant
  • Good electrical insulation
  • Easily weldable
Industry Applications:
  • Food processing industry
  • Chemical machines
  • Low load rollers

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 46.0 MPa6670 psiISO 2039-1
Tensile Strength, Yield 27.0 MPa3920 psi50 mm/min; DIN EN ISO 527-2
Elongation at Break 100 %100 %DIN 527
Modulus of Elasticity 1.06 GPa154 ksiDIN EN ISO 527-2
Charpy Impact Unnotched NBNBMax. 7,5j; DIN EN ISO 179-1EU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmDIN IEC 60093
Surface Resistance >= 1.00e+11 ohm>= 1.00e+11 ohmDIN IEC 60093
Dielectric Constant 2.4
@Frequency 100000 Hz
2.4
@Frequency 100000 Hz
DIN 53483
Dielectric Strength >= 40.0 kV/mm
@Thickness 1.00 mm
>= 1020 kV/in
@Thickness 0.0394 in
ASTM 149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C11.1 µin/in-°FDIN 53483
Specific Heat Capacity 1.80 J/g-°C0.430 BTU/lb-°FISO 22007-4:2008
Thermal Conductivity 0.410 W/m-K2.85 BTU-in/hr-ft²-°FISO 22007-4:2008
Melting Point 130 - 135 °C266 - 275 °FCrystalline; DIN 53765
Maximum Service Temperature, Air 80.0 °C176 °FLong term
 90.0 °C194 °FShort term
Heat Distortion Temperature 42.0 - 49.0 °C108 - 120 °FMethod A; R75
 70.0 - 85.0 °C158 - 185 °FMethod B; R75
Glass Transition Temp, Tg -95.0 °C-139 °FDIN 53765
Flammability, UL94 HBHBDIN IEC 60995-11-10
 
Descriptive Properties
ColorWhite / black / red / yellow / brown / green
Resistance to hot mater / basesResistant
Resistance to weatheringResistant in color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAID911 / 318872

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.