MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chi Mei Polylac® PA-717 General Purpose ABS Resin  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Melt Flow 6.4 g/10 min
@Load 3.80 kg,
Temperature 230 °C
6.4 g/10 min
@Load 8.38 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 44.0 MPa
@Thickness 3.17 mm
6380 psi
@Thickness 0.125 in
Elongation at Break 25 %
@Thickness 3.17 mm
25 %
@Thickness 0.125 in
Flexural Yield Strength 60.5 MPa
@Thickness 3.17 mm
8770 psi
@Thickness 0.125 in
Flexural Modulus 2.14 GPa
@Thickness 3.17 mm
310 ksi
@Thickness 0.125 in
Izod Impact, Notched  2.40 J/cm
@Thickness 6.35 mm
4.50 ft-lb/in
@Thickness 0.250 in
 2.78 J/cm
@Thickness 3.17 mm
5.21 ft-lb/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 199 °C390 °F
Middle Barrel Temperature 216 °C420 °F
Front Barrel Temperature 238 °C460 °F
Melt Temperature 232 - 260 °C450 - 500 °FNozzle temp not greater than stock
Mold Temperature 60.0 - 82.2 °C140 - 180 °F
Drying Temperature 87.8 - 93.3 °C190 - 200 °F
Dry Time 2 - 24 hour2 - 24 hour
Injection Pressure 68.9 - 82.7 MPa10000 - 12000 psi
Back Pressure 0.689 MPa100 psi
Screw Speed 50 - 60 rpm50 - 60 rpm
 
Descriptive Properties
Injection Fill SpeedSlow to Moderate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-717C ABS
Chi Mei Acryrex® CM-205 PMMA
Chi Mei Polylac® PA-757 ABS
Chi Mei Polylac® PA-747 ABS
INEOS Styrolution Terluran® GP-35 ABS

PLBZ00 / 50503

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.