MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Latamid 66 H2 K/20 PA 66, 20% Carbon Fiber Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Carbon Fiber Filled

Material Notes: Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/cc
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
Linear Mold Shrinkage, Transverse 0.0065 - 0.0095 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPa
@Temperature 150 °C
 105 MPa
@Temperature 120 °C
 115 MPa
@Temperature 90.0 °C
 140 MPa
@Temperature 60.0 °C
 200 MPa
@Temperature 23.0 °C
Elongation at Break 2.0 %
@Temperature 23.0 °C
 2.7 %
@Temperature 60.0 °C
 3.4 %
@Temperature 90.0 °C
 3.6 %
@Temperature 120 °C
 3.7 %
@Temperature 150 °C
Tensile Modulus 5400 MPa
@Temperature 150 °C
 7500 MPa
@Temperature 120 °C
 10000 MPa
@Temperature 90.0 °C
 14000 MPa
@Temperature 60.0 °C
 15500 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 45.0 kJ/m²
Charpy Impact, Notched 6.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 50000 ohm-cm
Surface Resistance 5000 ohm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
Vicat Softening Point 250 °C
@Load 5.00 kg
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 300 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized
Albis Plastics Polyamide 66 PA 910/1 CF 30 PTFE 15 , 30% Carbon Fiber, 15% PTFE, DAM
GEHR Plastics PA 6.6 Nylon 6.6, Conditioned

PLATH9725 / 177421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.